(Failed casting. At this point (3 castings) the mould was spent. If we used mould release/ graphene powder between each cast it would have lasted longer.)
 
(No difference)

Latest revision as of 17:08, 28 June 2019

Summary

Failed casting. At this point (3 castings) the mould was spent. If we used mould release/ graphene powder between each cast it would have lasted longer.

Licensing

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current17:08, 28 June 2019Thumbnail for version as of 17:08, 28 June 20193,648 × 2,736 (712 KB)Danspencer101 (talk | contribs)Failed casting. At this point (3 castings) the mould was spent. If we used mould release/ graphene powder between each cast it would have lasted longer.